Description
Mirror Finish, Any Surface: Achieve a stunning 95% reflective mirror chrome on any rigid or flexible material.
Feels Like Real Metal: Boasts a flawless shine and the tactile sensation of genuine metal plating.
Unrivaled Resistance: Excellent defense against abrasion, corrosion, UV light, temperature extremes, and harsh soiling.
Smarter Than Traditional Plating: A viable and simpler alternative to costly electro chrome plating, PVD, and UV photo-polymerization.
Easy Spray Application: Unlike conventional methods, it requires no investment in expensive coating equipment.
Fast Drying & Customizable: HLPV airless spray dries instantly and can be tinted with a transparent top coat for endless color and creative effects.
Code | TUTTOCHROMAME KIT STD TC20 Black primer | Unit Qty | Mix Ratio | COVER sqm/l |
TUT.PRI. IC100B | TUTTOPRIMER IC100B – black | 1 kg |
8-10 |
|
TUT.CAT. IC80 | TUTTOCATALYST IC80 | 0,8 kg | 80% | |
TUT.STD.TC20 | TUTTOCHROMAME STD TC20 | 1 L | ||
TUT.TOP.MT300 | CLEARTOP MT300 (Glossy finish) | 1 kg | ||
TUT.CAT. MT934 | CLEARCATALYST MT934 | 0,4 kg | 40%
|
TUTTOCHROMAME™ Application Guide
Follow these steps for a flawless mirror chrome finish:
- Prep Your Surface:
- Smooth It Out: For pitted areas, meticulously sand and level using medium to coarse grit sandpaper (400-600) to ensure maximum smoothness and flatness.
- Clean Thoroughly: Eliminate all contamination, especially on metal, with SCUDOPICKLING 100AB solvent cleaner.
- Apply the Primer:
- Mix it Right: Combine TUTTOPRIMER IC100B (100 parts) with TUTTOCATALYST IC80 (80 parts) at a 5:4 mix ratio.
- Spray Evenly: Apply using an HVLP spray gun (or standard spray gun) with a 1.2-1.3 mm nozzle at a pressure of 1.50 bar (21.75 psi).
- Shake Well First: Ensure both components are thoroughly mixed before use.
- Dry with Care:
- Oven Cure: Bake at 60°-70°C for 70 minutes, then let it cool and rest for 30 minutes.
- Air Dry: Allow to dry at ambient temperature (20-25°C) for 12-24 hours.
- Keep it Clean: Ensure drying occurs in a clean, dust-free environment. Avoid touching the coated surface during drying.
- Apply the Chrome:
- Shake Vigorously: Thoroughly shake the 1K TUTTOCHROMAME STD TC20 before pouring it into your HVLP spray gun.
- Spray with Precision: Use a 1-1.2/1.3 mm nozzle at a pressure of 1.50 bar (21.75 psi).
- Coat in Layers: Apply three even layers of TUTTOCHROME using overlapping, cross strokes to ensure complete coverage. A good technique is spraying bottom to top, then across from left to right.
- Dry for Maximum Shine:
- Oven Cure: Bake at 60°-70°C for 70 minutes.
- Air Dry (Optimal): For the best results and highest reflectivity (up to 90%-95%), allow to dry at ambient temperature for a full 24 hours. The longer the solvents evaporate, the better the mirror finish.
- Apply Top Coat:
- Mix the Clear Coat: Combine CLEARTOP MT300 (100 parts) with CLEARCATALYST MT934 (40 parts) at a 5:2 mix ratio using an HVLP spray gun (or standard spray gun) with a 1.2-1.3 mm nozzle at a pressure of 1.50 bar (21.75 psi).
- For Colored Finishes: If you desire a specific color, add CME Pigments to the mixed CLEARTOP MT300 and CLEARCATALYST MT934 according to the exact mixing percentages indicated on each CME Pigment bottle label.
- First Coat Drying: Let the first coat dry at 60°-70°C for 1 hour or at room temperature for 12-24 hours. After 3 hours, the coated item can be handled and packaged.
- Second Coat for Durability & Gloss: Always apply a second layer of the mixed CLEARTOP MT300 and CLEARCATALYST MT934 after any color coating. This ensures a high-quality, glossy, and long-lasting finish.
- For a Matte Finish: Instead of CLEARTOP MT300 and CATALYST MT934, use CLEARTOP MT800 (Matte finish) and SCUDO 8 SC Anti-fouling according to their specific mixing instructions.